Categories
Categories
Price: | US $ 8.9-13.55kilogram |
---|---|
Min Order: | 200kilogram |
Pay Type: | T/T,Western Union,Paypal |
Prod Model: | E-640 silicone for mold making |
---|---|
Color: | Translucent |
Feature: | Liquid |
Sample: | Available |
Purity: | 100% |
Certifications: | RoHS, MSDS, SGS, ISO9001:2000 |
Minimum Order Quantity: | 200 Kilogram |
Brand Name: | Hong Ye Silicone Rubber |
Place Of Origin: | Guangdong China |
Application: | Silicone Rubber for Mold Making |
Material: | Silicone Rubber |
Appearance: | Liquid |
Injection silicone for cystal diamond mold making
Description of injection molding silicone
Addition molding silicone is generally named two-components silicone
rubber, Part A and part B. It features an exceptional fluidity and good operability. The
mixing ratio is 1:1,mainly be suitable for making molds application.
Applications of injection molding silicone
Addition molding silicone could be mainly used for making concrete
Stones mold , resin jewelry mold , statue mold, artificial craft mold, wax molds, PU molds, resin molds, gypsum casting, candle molding and chocolate , candy and any other FDA food product mold making,prototyping , resin jewelry pendant ,etc.
Advantage of injection molding silicone
* low shrinkage (less than 0.1% )
*high tensile and tear strength with high copy times
*easy for operation (mixing ratio at 1:1)
*good fluidity easy for pouring operation ( in round 10000 cps )
Technique Data Sheet of injection silicone
Product | E-642 |
Appearance | Translucent |
Hardness(shore A) | 42±2 |
Mix ratio(A:B) | 1:1 |
Viscocity(mPa.s) | 12000±2000 |
Tensile strength (kgf/cm2) | 50±5 |
Tear-strength (kN/m) | 18±2 |
Elongation(%) | 450±50 |
Pot life/working time (mins) | 30-40 |
Curing time/setting time (hrs) | 3-4hrs(25°C) 110-20mins(60°C) |
Shrinkage rate (%) | ≤0.1 |
(Note: the hardness , color, curing time and operation time is adjustable)
Operation instruction of HY-E Series molding silicone:
1. Pls clear the model and tool totally before operation to prevent cure inhibition.
2.Weigh the two part correctly by electronic weight in two separate container .
3. Mixing the two part in 1:1 and stir part A and part B evenly in 2-3 minutes .
4.And get the mixture for vacuum-pumping for de-air the bubble in around 2-3
minutes . (If there is no vacuum machine, pls pour the mixture carefully and slowly
down the side of the mold frame so that less bubbles caused)
5. Enclose the product (the original model) with four plastic plates or wooden plates.
6. Clean your products and brush a layer of release agent(detergent or soap water) on
your product.
7. Pour the vacuumed mixture into the model frame from the side of the mold frame .
More information , pls feel free to contact Ms Hebbe:
Mob:+8618938861889