Molecular Sieve type 4A is an alkali alumino silicate; it is the sodium form of the Type A crystal structure. 4A molecular sieve has an effective pore opening of about 4 angstroms (0.4nm). Type 4A molecular sieve will adsorb most molecules with a kinetic diameter of less than 4 angstroms and exclude those larger. Such adsorbable molecules include simple gas molecules such as oxygen, nitrogen, carbon dioxyde and straight chain hydrocarbons. Branched chain hydrocarbons and aromatics are excluded.
Model | 4A | |||||
Color | Light gray | |||||
Nominal pore diameter | 4 angstroms | |||||
Shape | Sphere | Pellet | ||||
Diameter (mm) | 1.7-2.5 | 3.0-5.0 | 1.6 | 3.2 | ||
Size ratio up to grade (%) | ≥98 | ≥98 | ≥96 | ≥96 | ||
Bulk density (g/ml) | ≥0.72 | ≥0.70 | ≥0.66 | ≥0.66 | ||
Wear ratio (%) | ≤0.20 | ≤0.20 | ≤0.20 | ≤0.20 | ||
Crushing strength (N) | ≥35/piece | ≥85/piece | ≥35/piece | ≥70/piece | ||
Static H2O adsorption (%) | ≥22 | ≥22 | ≥22 | ≥22 | ||
Static methanol adsorption(%) | ≥15 | ≥15 | ≥15 | ≥15 | ||
Water content (%) | ≤1.0 | ≤1.0 | ≤1.0 | ≤1.0 | ||
Typical chemical formula | Na2O . Al2O3. 2SiO2. 4.5 H2O | |||||
Typical application | a) Drying and removing of CO2 from natural gas, LPG, air, inert and atmospheric gases, etc. | |||||
Package | Carton box; Carton drum; Steel drum | |||||
MOQ | 1 Metric Ton | |||||
Payment terms | T/T; L/C; PayPal; West Union | |||||
Warranty | a) By National Standard HGT 2524-2010 | |||||
b) Offer lifetime consultation on problems occurred | ||||||
Container | 20GP | 40GP | Sample order | |||
Quantity | 12MT | 24MT | < 5kg | |||
Delivery time | 3 days | 5 days | Stock available |
Molecular sieve Type 4A can be regenerated by either heating in the case of thermal swing processes; or by lowering the pressure in the case of pressure swing processes.
To remove moisture from a 3A molecular sieve, a temperature of 200-230°C is required. A properly regenerated molecular sieve can give moisture dew points below -100°C.
The outlet concentrations on a pressure swing process will depend on the gas present, and on the conditions of the process.
To avoid damp and pre-adsorption of organic before running, or must to be reactivated.